I am posting this here because I think it may have something...
- Jul 27, 2012
by
Patrick
I'm with you on microcracking. The best way to confirm this ...
- Jul 30, 2012
by
davef
I would look at your de-paneling process. How are you cutti...
- Aug 22, 2012
by
Reese
They are using the method where scored boards are separated ...
- Aug 22, 2012
by
Patrick
Most likely the depaneling is not your issue, but I do concu...
- Aug 22, 2012
by
Reese
I also forgot to mention that the pizza-slicers you are usin...
- Aug 22, 2012
by
Reese
"The problem is we haven’t changed anything in our design, a...
- Aug 23, 2012
by
isd.jww
Moisture should not be an issue with ceramics, but mechanica...
- Aug 27, 2012
by
Th. Meier