Greetings everyone,
I am trying to figure out away to clean...
- Aug 03, 2012
by
Zana
Not the best situation in the world, but you know that.
C...
- Aug 03, 2012
by
davef
You might want to look at a hand held ultrasonic stencil cle...
- Aug 06, 2012
by
Jeremy
Thank you Dave,
As always you provide us valuable informat...
- Aug 06, 2012
by
Zana
Thank you Jeremy,
That might be the solution. I will conta...
- Aug 06, 2012
by
Zana
Techspray makes a liquid called "Eco-Stencil SMT Stencil Cle...
- Aug 06, 2012
by
dyoungquist
wipes + IPA (isopropyl alcohol) can bring good result to you...
- Aug 07, 2012
by
ENIAC
Thank you for all your inputs,
I was thought not to use alc...
- Aug 07, 2012
by
Zana
I would advise against using IPA for stencil cleaning It m...
- Aug 17, 2012
by
Jeremy
Zana