Does anyone have any input on ESD Epoxy flooring, positive o...
- Jun 19, 2013
by
ehess
I've used it at my last two companies, and quite like it. T...
- Jun 19, 2013
by
robgd3
were you forced to reapply over time? thanks for the input....
- Jun 19, 2013
by
ehess
We only reapplied in areas where significant wear was observ...
- Jun 19, 2013
by
robgd3