We have a 0603 film chip capacitor defined by mfgr as "stack... - Jun 05, 2014 by SWAG
If your TAL is 90 sec, and the mfg spec is ">230C for max 30... - Jun 05, 2014 by isd.jww
Good observation. I don't believe so as we reach 225 C for ... - Jun 05, 2014 by SWAG
Can you see the flaking right out of the oven? ... - Jun 06, 2014 by isd.jww
Component manufacturers subject their lots to thermal / refl... - Jun 06, 2014 by SteveO
Yes, jsd.jwww it can be seen right after reflow. I read bac... - Jun 09, 2014 by SWAG