Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3963
What could be the possible solution for shorted BGA but only...
- Dec 22, 2014
by
slouis2014
the most common reason can be popcorning of the device or wa...
- Dec 23, 2014
by
Bob Willis
The peak temp. during reflow is 285 degree, at this temperat...
- Dec 23, 2014
by
slouis2014
Assuming its 285 Celsius as measured at the solder joint, yo...
- Dec 24, 2014
by
JimPat
285 is way too high a temperature for a measured part or bal...
- Dec 24, 2014
by
Bob Willis
thanks for all the information. i will check on it.
...
- Dec 28, 2014
by
slouis2014