Hi all, Am new to SMT here. I have a very thin laminat... - Jan 26, 2017 by Joshua Goi
Consider that printing may not be the only approach to getti... - Jan 27, 2017 by davef
> Hi all, > > Am new to SMT here. > > I... - Jan 30, 2017 by Robl
so, why are your laminates warped? What needs to be done to ... - Jan 30, 2017 by davef
Thanks Rob. I'm not so sure in a mass production environm... - Jan 30, 2017 by Joshua Goi
I just assume when you have laminates that thin, it will inv... - Jan 30, 2017 by Joshua Goi
Tacsil is another product you might try. ... - Jan 30, 2017 by SWAG
Looks like a similar product to magic resin. Thanks I'll ... - Jan 30, 2017 by Joshua Goi
Hi Joshua, We ran 150K per week this way, you just need ... - Jan 31, 2017 by Robl
Hi Rob, So do you have to constantly remove the old adhes... - Jan 31, 2017 by Joshua Goi
Dispensing: You can dispense for 0201 and above Warped la... - Jan 31, 2017 by davef
Hi Joshua, No, the adhesive lasts 2 or 3 runs. The adhes... - Feb 01, 2017 by Robl