Hi everyone. We use a small ultrasonic aqueous cleaner. Aft... - Dec 27, 1999 by RICK_EEI
If it's what I think it is you have a white residue on the ... - Dec 27, 1999 by
Depending on the components you are seeing this on, one t... - Dec 27, 1999 by
I have tried the water soluble flux and the aqueous cleaner... - Dec 28, 1999 by Amy Castor
Rick, Does the ultrasonic cleaning system that you use reus... - Dec 28, 1999 by Christopher Lampron
Rick, Ultrasonics is a mechanical scrubbing action (cavitat... - Dec 28, 1999 by Frank Grimard
Hi Rick, Water soluble flux is heatee, deionized water. So... - Dec 28, 1999 by Jim
Rick, The first line of my message should have read as: "... - Dec 28, 1999 by Jim
Moving water will disrupt the ultrasonic cavitation. If yo... - Dec 29, 1999 by Frank Grimard
Intel had a similar problem with one of their military pack... - Dec 31, 1999 by