So i am a quality inspector and i am having issues with the ... - Aug 04, 2017 by Adonys Bruno
What are the vias somewhat filled with? Can you explain in g... - Aug 04, 2017 by davef
Hi Adonys, Can you attach the photo for check? ... - Aug 04, 2017 by Dawson
The vias are filled with the silver plating, it's excess pla... - Aug 07, 2017 by Adonys Bruno
Are you seeing this on bare PCBs or after assembly? with ... - Aug 07, 2017 by dwl
I agree. Just thinking.. could it be copper plating issue... - Aug 09, 2017 by Stivais
I would recommend that you have some of the subject vias mic... - Aug 09, 2017 by EdHare
I am trying to get a picture from my manager because its ver... - Aug 09, 2017 by Adonys Bruno
Here are some of the issues im having. 1. is the Dark Vi... - Aug 10, 2017 by Adonys Bruno