PCB assemnly cost analysis | 14 November, 1999

I would like to know all the information about PCB assembly cost analysis. Anyone who has the information or know the source, please show me. I am very preciate about it.. The information can be Software, book, magazines, forum, and technical documents. Thank you.

reply »

#8536

Re: PCB assemnly cost analysis | 15 November, 1999

Tuan: Many people develop spreadsheets to represent their processes and costs. Also, check out CostCoach at http://www.costcoach.com, it may be just what you need. It was developed by Phil Zarrow, Ron Lasky of MPM, Dr. Dan Baldwin of Georgia Tech and Jessica Lasky at Purdue, and can approach assembly quoting from a multitude of angles.