Hello, Looking for some insight. We just finished a run a... - Nov 10, 1999 by
Hi Dave Sounds like what we call a "squeeze ball". Usually ... - Nov 10, 1999 by John Thorup
Hi, Dave Which brand of solder paste are you using? Is it ... - Nov 10, 1999 by
For me it sounds like to much paste. If it worked in former... - Nov 11, 1999 by Wolfgang Busko
Dave: I think you�re correct. The solder balls are probab... - Nov 11, 1999 by davef
Dave Vulcano