SERA and ROSA | 5 November, 1999

Anyone have information on the ROSA Technique? It is a derivative of the SERA analysis for solder-ability on pads, (they are not italian sisters)I belive the techniques were developed by Rockwell and Motorola.

thanks in advance. JKK

reply »

#8657

Re: SERA and ROSA | 8 November, 1999

Reduced Oxide Soldering Activation is an electrochemical method of restoring the solderability of surfaces. Searching the archives of IPC technet and this forum will reveal more details. John Thorup

reply »

#8658

Re: SERA and ROSA | 9 November, 1999

Jeff: Try this:

ROSA. John�s spot on. I�ll add that it is a fluxless method that reduces the oxides in an aqueous solution. Another source of information is: Trench, M., Hillman, D., Lucey, G., "Environmentally Friendly Closed Loop Soldering," 1993 International CFC And Halon Alternatives Conference, Washington, DC. ROSE. Resistivity of Solvent Extract. A non-destructive technique contamination measurement technique that washes a IPA / DI water solution over a board and compares the resistivity of the solution to an equivalent NaCl solution to estimate ionic material. SERA. Sequential Electrochemical Reduction Analysis. A non-destructive technique that characterizes solderability, surface metal oxides, and intermetallics. SERA looks at surface oxidation in a much more user friendly manner that SEM or Auger.

Good luck