Hello, Could you please tell me if there is any industry ... - Mar 26, 2019 by Hypnotia
There is no "industry standard" that I am aware of. Ideally,... - Mar 26, 2019 by charliem
Charliem, Thank you for the input. Following this logi... - Mar 27, 2019 by Hypnotia
200uM seems high. I say this because typically our solder ... - Mar 27, 2019 by charliem
There is no industry standard for BTC stand-off height. "... - Mar 28, 2019 by davef
Davef, Thank you for the comprehensive reply. I do really... - Mar 28, 2019 by Hypnotia
Yes, No standard.Normally QFN supplier suggest 50-75 um (2-3... - Jul 01, 2019 by sssamw
We have seen that vias included in the PCB under the thermal... - Jul 03, 2019 by SMTA-Pat SMTA