When baking parts at 90C that require 15 hours bake time wit...
- Sep 19, 2019
by
QAnalyst1
Briefly opening the door probably won’t affect anything sign...
- Sep 19, 2019
by
DeanM
Thank you for the response, yes, the oven is vented. I guess...
- Sep 20, 2019
by
QAnalyst1
It won’t hurt’em if under 96 hrs.
...
- Sep 20, 2019
by
DeanM
Very good. Thanks.
...
- Sep 20, 2019
by
QAnalyst1