Hej, we have some connectors placed on our PCB. 2*30legs 0... - Jan 16, 2020 by Soupy
Hej back at ya Your connectors could be warping during refl... - Jan 16, 2020 by davef
Thanks Dave, We have avoided rotating the board as it is so... - Jan 17, 2020 by Soupy
Try preheating the connectors ... - Jan 17, 2020 by davef