IPC calls out 100% wetting to land. I need to understand why... - Apr 17, 2020 by QA123
A-610G 7.5.16 Components with Bottom Thermal Plane Terminati... - Apr 19, 2020 by davef
A-620G doesn't require 100% wetting to the thermal pad. It r... - Apr 19, 2020 by davef