Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4287
Hi,
We are currently using WonderMask PX Peelable Solder M...
- Apr 22, 2020
by
MVARGAS
We prefered kapton tape to peelable mask, though, there is a...
- Apr 22, 2020
by
robgd3
We use Wondermask 2211 and we haven't had issues with the ma...
- Apr 22, 2020
by
SMTA-Samy
SMTA
Hi, thank you both for answering. Unfortunately, due to volu...
- Apr 23, 2020
by
MVARGAS
Is your board spending 40s on a molten solder at 500F?
...
- Apr 27, 2020
by
Evtimov
That's correct. This is because the component (switch) needs...
- Apr 27, 2020
by
MVARGAS
Are you watching for copper dissolution?
At one place I was ...
- Apr 28, 2020
by
Stephen
PCB Electronics Ltd, a leading corporation focusing on one-s...
- Apr 29, 2020
by
Tomzhao2