Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 1793
Looking for CTE and young's modulus values for aluminum back... - Jun 04, 2020 by SMTA-Robert SMTA
The typical CTE below Tg is 40 ppm/K and 110 above Tg ppm/K.... - Jun 24, 2020 by SMTA-Dave SMTA