We are currently producing a project that brings a TQFP64.
B...
- Apr 16, 2021
by
Sebas
I'm concerned by the solder spheres in the via on the first ...
- Apr 16, 2021
by
DWL
I agree with DWL's comments. Also, your profile is really re...
- Apr 20, 2021
by
kyleh04
Solder balls, can be excess paste by opening ST.