Hello!
Anyone here knows is there any specific time frame (...
- Apr 14, 2022
by
Evelyn
depends on board finish and PCB substrate materials. If you ...
- Apr 14, 2022
by
cbart
Thank you for sharing the helpful information.
Let's say th...
- Apr 15, 2022
by
Evelyn
Bake a board. Measure weight. Measure board weight that have...
- Apr 15, 2022
by
Evtimov
So you run one side, and leave the boards sit in temperature...
- Apr 18, 2022
by
ProcEng1
Be aware that some "water soluble" fluxes can be c...
- Apr 18, 2022
by
charliem
Be careful of MSL level 4 or higher devices on the first sid...
- Apr 19, 2022
by
DWL
Alright. Thank you Evtimov :)
...
- Apr 20, 2022
by
Evelyn
@ProcEng1
Yea. Mostly is ENIG surface finished PCB. Sometime...
- Apr 20, 2022
by
Evelyn
@charliem,
For the clean process board using "water...
- Apr 20, 2022
by
Evelyn
@DWL, Roger that. Thank you for your advice :)
...
- Apr 20, 2022
by
Evelyn