Flux on the body of SMT components

Views: 1177

#90637

Flux on the body of SMT components | 28 February, 2024

Hello all,

I have a flux over components that affects AOI results in reading the symbols on top of it. What would you recommend to minimize this effect?

Attachments:

reply »

#90639

Flux on the body of SMT components | 28 February, 2024

Find out were the excess flux is coming from. See if it can be eliminated or reduced at the source. Lokely coming from something other than SMT assembly.

reply »

#90640

Flux on the body of SMT components | 28 February, 2024

I have seen there is flux like stuff dripping off from the exhaust area of the reflow oven onto the board That would be the issue of poor maintenance.

reply »

#90687

Flux on the body of SMT components | 13 March, 2024

The image is very poor.

I would start with giving the oven a good clean. You likely have some build up that is then dropping onto your boards causing this.

reply »