I'm having a lot of trouble placing a long thin connector (D... - Aug 06, 2024 by Poly
Poly, I don't know the UIC GX11 but on other machines I wou... - Aug 06, 2024 by jdengler
We are working with ASM SX machines. To solve similar issues... - Aug 07, 2024 by Dima
Perhaps moving this connector to the end of the placement se... - Aug 19, 2024 by griinder
I would also consider the smount of solder paste. If it can ... - Aug 22, 2024 by SMTA-69549243 SMTA