lead free dip or cream solder | 19 August, 1999

we've received an inquiry if lead free solder for solder dips or surface mounting (cream solder) is available on a technical scale

reply »

#10044

Re: lead free dip or cream solder | 19 August, 1999

| | | we've received an inquiry if lead free solder for solder dips or surface mounting (cream solder) is available on a technical scale | Dr. Weber I'm not sure what you mean by "on a technical scale" but various no lead alloys are available in most forms from many if not all of the major players. Aim, Alpha and Indium jump to mind. Try accessing the new IPC no lead forum.| Hope this helps John Thorup |