| My engineering Dept. has informed me that they want | to start using pins, on an aluminum substrate in the | smt process. Pins are interconnect for daughter bds. | Dia. of pins 0.020" 0.040" 0.080" flat bottoms | 1) Does any one know how to hold pins in place during | REFLOW? | 2) Is there a way to automate this process? | | Please advise....THANKS | You could put a machined "cap" over all pins, holding them all together in place. If the cap is not too large it could be placed by the machine after placing the pins.
reply »