Hi,

would like to get good info on the above solder paste metal content regarding their advantage and disadvantage against each other and their effect on fine pitch solderability.

regards,

reply »

#17200

36PB/62Sn/2Ag Vs 63Sn/37Pb | 14 August, 2001

2% silver will be a little shinier. [Some inspectors hate that.] After that differences get murkier.

Some people believe that 2% silver does something er other to scavange gold and silver to produce a less brittle connection. We have never seen evidence of that.

reply »

mugen

#17201

36PB/62Sn/2Ag Vs 63Sn/37Pb | 14 August, 2001

Basic understanding,

1) the 2% silver (Ag) gives better shine *joint surface*.

2) Ag improves stength & fatigue resistance of solder joints

3) reduces leech-out of silver from silver-base substrates (eg of such silver-base surface contact: metallized faces of CAP & RES)

4) Extract from a book:

Sn63/Pb37 Tensile Strength : 4.0 tons/sq.inch @20 deg-C Elongation : 50%

Sn63/Pb35/Ag2 Tensile Strength : 4.2 tons/sq.inch @20 deg-C Elongation : 40%

This means better mechanical performance....

Caution : monitor that ur paste has no more than 2% Ag, too much of a good thing can kill.....

Inquire with your paste supplier(s), and compare their technical discussion details....

reply »

#17202

36PB/62Sn/2Ag Vs 63Sn/37Pb | 14 August, 2001

Say isn't creep a more key issue, rather than strength?

reply »

mugen

#17203

36PB/62Sn/2Ag Vs 63Sn/37Pb | 14 August, 2001

true.... tata why the elongation% is there.....

reply »

#17204

36PB/62Sn/2Ag Vs 63Sn/37Pb | 14 August, 2001

But isn't elongation more of a quantification of ductility than of creep?

reply »

mugen

#17233

36PB/62Sn/2Ag Vs 63Sn/37Pb | 16 August, 2001

Say din't someone previously claim, "Dave F" stands for :

Damm.Averted.Verified.Eggbrain.Freakin *smart* ?!?

reply »

#17248

36PB/62Sn/2Ag Vs 63Sn/37Pb | 16 August, 2001

Just feel relieved that we didn't go to the matt on the use of "leaching" rather than "dissolution".