Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
when taking a reflow profile, can i attach the thermalcouple...
- Sep 21, 2001
by
You can, and for small parts you probably won't see much dif...
- Sep 21, 2001
by
Steve Thomas
You can measure temperatures any place that you would like, ...
- Sep 21, 2001
by
davef
We're used to placing the theromcouple on the solder joint a...
- Sep 21, 2001
by
We like that method for certain jobs. The res sometimes fre...
- Sep 22, 2001
by
davef
Back-stepping a bit. If a profile is being used to:
* Set-...
- Sep 22, 2001
by
davef
I like to secure the thermalcouples with a small dot of chip...
- Sep 22, 2001
by
there is a company called EFD. my contact there is john kami...
- Sep 26, 2001
by
bobm
does EFD have a website?
-vance
...
- Oct 09, 2001
by
check out ECD.com for temprobes.
...
- Oct 09, 2001
by
random7
THE PEOPLE THAT MAKE THE PROFILING EQUIPMENT IS. ECD. THERE ...
- Oct 09, 2001
by
bobm
steven