Dear sir, Do you have experiment about the temperature cycling and vibration test for reliability testing of surface mount solder attachment. If yes, please give me the soft file sample of parameter setting and testing report.. Thank you very much. Best Regards, Sanchai.K

reply »

#19434

Temperature cycling | 9 April, 2002

Read SM-785 - "Guidelines For Accelerated Reliability Testing Of SM Solder Attachments"