Hi,

Does anyone know about if there is any specs of Lead free Joint Strenght by IPC or from Japan?

We are Starting a evaluation shortly and should be lead free by February 2003

Regards, Mr.T

reply »


CAL

#20255

Lead-Free | 6 June, 2002

I have not seen any, but that does not mean they do not exist. I do know lead-free is starting to loose its momentum. Compliance dates are being pushed back. And also some of the European standards developments are starting to make exceptions (i.e. military electronics or Hi-rel) to the compliance dates and specs. I know there are companies out there working on reliability issues but more for internal preparation.

CAL

reply »

#20256

Lead-Free | 6 June, 2002

While loosing traction, lead-free is a fait accompli. The 'greens' rule Euroland and the rest are sheep, too fat and content to realize what's happening.

While not addressing your question on strength directly, National Electronics Manufacturing Initiative (NEMI) in Herndon, VA recently published a report on the reliability of lead-free solder connections. Look here: http://www.nemi.org/PbFreePUBLIC/index.html

'Enough jibba jabba.' You are one of my favorite TV personalities. 'Shuddup foo.'

reply »

Mr.T

#20270

Lead-Free | 7 June, 2002

Thanks for answers....In Euroland (My place)it is not so clear.And this is confusing: There is 3 different comittee�s in Europe. First says 1 of January 2007.Second says 1 of January 2006, and third one says that any of these will do.

Also we get a pressure from our customer and they want to be lead free.

Thanks, Mr.T "I pity the fool"

reply »

#20275

Lead-Free | 7 June, 2002

Kay Nimmo [ http://www.itri.co.uk/soldleg.htm ] knows what's happening. Ask her to tell us.