any of you guys got any ideas to clear up this stuff of the ...
- Jun 13, 2002
by
EricD
An ounce of prevention is worth a pound of cure. Why not fi...
- Jun 13, 2002
by
davef
well as usual this for flip chip however, this application u...
- Jun 15, 2002
by
EricD
Consider slowing down the rate of heating during reflow to e...
- Jun 17, 2002
by
davef
mebbe you can try to Kapton Tape the nearby gold pads that a...
- Jun 19, 2002
by
ianchan
thanks yeah we are very much looking at the reflow because t...
- Jun 20, 2002
by
EricD
EricD