Hello there:
1- I know someone who diluted expired solder paste, which obviously lost its tackiness using Isopropanol. The paste was expired by more than 6monthes but after dilution I saw by myself the paste has retrieved its tackiness. The amazing result of solder joints I saw under the microscope made me ask you if there is a standard for doing this. I have scrapped a lot of paste before and I hoped there could be a way to avoid loosing all that money.
2- On what basis should I replace the metal squeegee blade? We have a DEK 248, which ran more than 100K of prints without changing the squeegee blade, is it the time to be replaced? What are the criteria?
Thanks everyone. Hany