PCB finish requirement for COB process

andy

#21737

PCB finish requirement for COB process | 24 September, 2002

For the COB process, what thickness for plating Au is suitable? IS there any specification for this issue?

reply »

andy

#21738

PCB finish requirement for COB process | 24 September, 2002

we used the ball bonding, just normal chip on board.

as I know the the electroless Ni/immersion Au, the gold thickness is about 0.13um at most, what about chemical plating or electrolytic plating?

any experience on it, thanks

reply »

POC

#21778

PCB finish requirement for COB process | 27 September, 2002

I spec COB using wire bond attach - 0.75um � 0.25 Gold over 5um � 3 Nickle.

reply »

#21780

PCB finish requirement for COB process | 27 September, 2002

Mar,

The previous post makes the best point. Your finish spec depends on the COB process you plan to use. Is your process: * Gold wire bond * Aluminum wire bond * Flip chip * Er, watt