Hello everyone out there in the SMT world. I have a dilema ...
- Sep 26, 2002
by
Abelardo Rodriguez
unsure of what solder spec. your working to?.IPC/EIA J-STD-0...
- Sep 26, 2002
by
Both you and a previous poster are correct. Grainy / shiney...
- Sep 26, 2002
by
davef
Is there a steadfast rule of thumb for a good solder joint o...
- Oct 02, 2002
by
Have you had your solder pot tested? I find that levels of c...
- Oct 02, 2002
by
Steven
The steadfast rule of thumb is: In order to get reliable ref...
- Oct 02, 2002
by
davef
Abelardo Rodriguez