Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
we have recently been trying silver composition on our pads ...
- Jan 15, 2003
by
burb1999
Grainy finish of the solder joint also caused by higher refl...
- Jan 15, 2003
by
Vijay
Grainy finish of the solder joint also caused by higher refl...
- Jan 15, 2003
by
Vijay
I have been using silver coated boards for over 3 years and ...
- Jan 16, 2003
by
Lee
I have heard that the profiles are pretty much the same but ...
- Jan 16, 2003
by
burb1999
Hi burb , reflow temps are same than other profiles just fol...
- Jan 16, 2003
by
Hi Burb,
I think you should try with paste which consist Ag...
- Jan 20, 2003
by
Evtimov
I fyour just using Sn/Pb in your paste even using nitrogen w...
- Jan 24, 2003
by
JohnW
Hi
Don't really know what "your grainy" means. It could b...
- Jan 24, 2003
by