Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
I seem to recall seeing some references to controlling the t... - Jan 20, 2003 by Steve Thomas
Double check the data sheets for your paste. Just as an exa... - Jan 20, 2003 by Jon Fox
Sorry, what I meant was that they don't provide a duration f... - Jan 20, 2003 by Steve Thomas
Hi Stevo, Most paste suppliers say something like, �above... - Jan 20, 2003 by davef
Hi You already received good answers. A thing to remem... - Jan 21, 2003 by
OK, so the issue is with the variability of the alloys on th... - Jan 21, 2003 by Steve Thomas
Hi I thought I would come back to this one for a second. ... - Jan 22, 2003 by