Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
DO YOU KNOW? WHAT KIND OF SOLDER PASTE IS BETTER IN ORDER TO... - Mar 11, 2003 by
Some people have said that for smaller components like 0402,... - Mar 11, 2003 by genny
Ditto on the profile/reflow oven...a couple years ago, we ha... - Mar 13, 2003 by mr
Hi, About Thombstone defects: 1.Placement accuracy-main re... - Mar 14, 2003 by Evtimov
Hi I got thinking about this and did some reading. Fir... - Mar 14, 2003 by
Hi, We had tomb-stoning on a product, and it was quite se... - Mar 15, 2003 by
Hi Good, that is one of the things I see some have done. ... - Mar 16, 2003 by
I like this answer! Part geometry, part mass, land patter... - Mar 18, 2003 by Steve Thomas
Here is what I have been finding lately. We switched to a 2... - Mar 18, 2003 by RDR
Hello Garcia: For my experience in Tombstone problems I r... - Mar 20, 2003 by
Hi I understand that more circular or rounded pads also r... - Mar 20, 2003 by
Hi Rene Great, I am glad to see that you are recommending... - Mar 20, 2003 by
additonally, minimizing the rising rate aroud 183'c and decr... - Mar 27, 2003 by
Hi kenlchin, Yes, This all helps with these little com... - Mar 27, 2003 by
can any one tell me if you should run the same heat on the ... - Mar 27, 2003 by
Just to be sure, you really should. PCB thickness and compo... - Mar 27, 2003 by Jon Fox
Hi I hope I am replying in the correct tread down link. ... - Mar 27, 2003 by
Hi, Look there are some important factors.The height is fir... - Mar 28, 2003 by Evtimov
Hi Yes I agree, yet this subject is about Tombstoning and... - Mar 28, 2003 by
Hi All, The best solution we made on our tombstone defect... - Apr 04, 2003 by Alex Yalung