Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hello,all.these days I met many skewed transistors after ref...
- Apr 18, 2003
by
tsongshe
Transistors? Are you referring to SOT-23 packages?
Are the ...
- Apr 18, 2003
by
k_h
Here's how Kevin posted his pix ...
- Apr 18, 2003
by
davef
I'm sure the parts and solder paste are well registered.
th...
- Apr 18, 2003
by
tsongshe
Thanks Dave.F.
I 've carefully read what you recommended,bu...
- Apr 18, 2003
by
tsongshe
Brian
What did we recommend? We just gave you a link so ...
- Apr 18, 2003
by
davef
"glue the floater in place with chip bonder before reflow"
...
- Apr 18, 2003
by
Steve Thomas
Thanks.
*We use TO252 package,but sometimes the skewed comp...
- Apr 20, 2003
by
Hi,all,
I'm very glad here this site to meet so many fri...
- Apr 20, 2003
by
Your link doesn�t work. It gives an application timed out m...
- Apr 20, 2003
by
davef
Thank you Dave F
...
- Apr 21, 2003
by
You might try reducing your solder paste volume. To much sol...
- Apr 21, 2003
by
k_h
I remember from my days of machine setups that these package...
- Apr 21, 2003
by
Jon Fox
I'll throw this out there also:
...
- Apr 22, 2003
by
k_h
I think it will make some progess if you modify the program ...
- Apr 23, 2003
by
jedduan
tsongshe