Does anybody have any advice on how to get a decent profile ... - May 14, 2003 by brad
Unless you have a reason, set your top and bottom to the sam... - May 15, 2003 by davef
Hi, I can give you a few steps. 1. The solder paste. Take... - May 19, 2003 by Evtimov
Dave, We are using Kester Easy Profile 256 No clean Sn62P... - May 19, 2003 by brad
Curious. Are you finding no applications support from Dima o... - May 19, 2003 by PeteC
How are you attaching your thermocouples? When using HT... - May 20, 2003 by EnthDegree
Something else to keep in mind when you reflow using an I... - May 21, 2003 by
Cameron, I am burying the thermocouple in high temp solder ... - May 23, 2003 by brad
Hi, I think using a epoxy glue will be a more approriate... - May 23, 2003 by Kris