Can anyone help? We need a PCB material capable of working at 200 deg C, we are currently using Norplex P95 but we are being stung with huge minimum order quantites as we are in the uk and all the manufacturers have to buy it in on special order. Does anyone know of another material with similar properties that would be more readily available in the UK. We have tried Arlon 85N and this has proved more difficult to get hold of than the P95.

reply »

#25635

High temp PCB material | 3 September, 2003

Dunno about UK suppliers, how about: * Isola P97 / P27 * Polyclad GI-787

If laminates are so bloody expensive in UK, why not them have made in the States?