Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
I am having a problem with SOT23 moving off their pads durin...
- Sep 16, 2003
by
James,
Could it be the convection in the reflow oven itself...
- Sep 16, 2003
by
Hi James,
is it your oven a convection forced air ?
i...
- Sep 16, 2003
by
We do have a convection oven and no one has messed with it. ...
- Sep 16, 2003
by
Medium should be fine,is it only one particular reference de...
- Sep 16, 2003
by
mantis
It is one reference designator by a Tant C cap. When I look...
- Sep 16, 2003
by
For some reason I cant claim your email to send you mine. I...
- Sep 16, 2003
by
Also most of Tantalum Caps are iron-magnetic material made, ...
- Sep 16, 2003
by
How consistant is it? If it is every board try sending one t...
- Sep 16, 2003
by
interesting!
I recently invested a small personal fortun...
- Sep 16, 2003
by
Are there via's underneath the Tantalum, closed with solderm...
- Sep 17, 2003
by
Check the tant cap for outgassing, tant caps are notorious f...
- Sep 17, 2003
by
James
Hi all,
by reading along those thread (SOT23) and Tan outga...
- Sep 18, 2003
by
Thanks to everyone for replys. I have to agree. I will have...
- Sep 19, 2003
by
James