Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
I'm looking at an application that would require 62/36/2 sol...
- Oct 15, 2003
by
It is a direct switch over from what I have experienced. Yo...
- Oct 15, 2003
by
RDR
We agree with Russ
...
- Oct 15, 2003
by
davef
You will also find an increase in the costs of the paste
...
- Oct 15, 2003
by
LarryK
Wettability also will increase, so it could generate briges ...
- Oct 15, 2003
by
Gabe, Interesting, I have never encountered that before. Wh...
- Oct 15, 2003
by
RDR
Can also reduce leaching of certain types of components.
...
- Oct 15, 2003
by
DL
I have only used this on Mov assy's, never on boards. If usi...
- Oct 15, 2003
by
adlsmt
Russ, you are right, I've seen briging on 16 mils pitch on O...
- Oct 16, 2003
by
John