Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi,
I have a soldering problem with a header SMT straight...
- Nov 17, 2003
by
When the pads on the board are too large, the component tend...
- Nov 22, 2003
by
davef
Dear Frank,
could it be that your component legs are coated...
- Dec 02, 2003
by
Frank