Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
We are having problems removing the flux residue from our bo...
- Feb 18, 2004
by
jdumont
You have two choices� Change your paste or beef-up your was...
- Feb 18, 2004
by
I actually have Kyzen's Aquanox 4520 in there now. Trace Mel...
- Feb 18, 2004
by
jdumont
Is this a white residue on the joint and surrounding area's,...
- Feb 23, 2004
by
Is this a white residue on the joint and surrounding area's,...
- Feb 23, 2004
by
Is this a white residue on the joint and surrounding area's,...
- Feb 23, 2004
by
Why are you cleaning a NC solder paste?
...
- Feb 23, 2004
by
We clean some of our boards because we are in the medical an...
- Feb 24, 2004