tombstoning (leadfree solder paste) | 15 July, 2004

WERW HAVING PROBLEM IN OUR PRODUCT SINCE WE STARTED USING A LEADFREE SOLDER PASTE..REJECTS OF TOMBSTONING IS SO ERRATIC...HOPE YOU CAN GIVE SOME INPUTS HOW TO CONTROL THIS..WHAT IS THE POSSIBLE CAUSE?THANKS

This message was posted via the Electronics Forum @

reply »

#29515

tombstoning (leadfree solder paste) | 15 July, 2004

Get started by searching the fine SMTnet Archives. We love talking about tombstoning and solderballs. Good luck.