Hi
How does one distinquish between hard gold and immersi...
- Aug 11, 2004
by
Q1: How does one distinguish between hard gold and immersion...
- Aug 11, 2004
by
davef
This is interesting, I was once told by a PCB supplier that ...
- Aug 12, 2004
by
RDR
Russ: Immersion gold [imm Au] is "soft" and it's "gold", but...
- Aug 12, 2004
by
davef
Hi Guys
thanks for the replies.
Dave, the spec is no...
- Aug 16, 2004
by
You bet our reponse changes.
Q2R: Hard gold thickness is ...
- Aug 16, 2004
by
davef
what about areas that are soldered ?
This is def not a E...
- Aug 16, 2004
by
As we mentioned in an earlier response in this thread [Q5], ...
- Aug 16, 2004
by
davef
ok I agree there has been a confusion with terminology
Wh...
- Aug 16, 2004
by
First, we didn't say "electrolytic soft gold with a minimum ...
- Aug 16, 2004
by
davef
thanks all
...
- Aug 19, 2004
by
Kris