Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
I use conformal coating DYMAX #984-LVUF and I don't know if ... - Feb 17, 2005 by Frank R.
We're not familiar with your DYMAX #984-LVUF. The problem is... - Feb 17, 2005 by davef
Thanks Dave, The problem is on all 0805. Do you think it... - Feb 18, 2005 by Frank R.
It's weird that it would be just 0805. When we see this it ... - Feb 18, 2005 by davef
Frank R, I believe the Dymax #984-LVUF is a POLYURETHANE RE... - Feb 18, 2005 by JRL
Dave, Few questions concerning your Umiseal 1B73. To c... - Feb 23, 2005 by Frank R.
We: * Cure 1B73 according to spec in a heat box, like a Blu... - Feb 23, 2005 by davef
Some UV cure coatings do not have the correct rheology for s... - Mar 21, 2005 by sforman1
Normally, some conformal coatings do not have very good wett... - Apr 10, 2005 by
The solid content of 1B73 is too low, especiall when you add... - Nov 23, 2006 by