Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Hi,
Actually, we want to run a benchtest for solder paste...
- Mar 01, 2005
by
ING
Indium NC SMQ92J for both lead and unleaded
...
- Mar 01, 2005
by
RDR
Cookson solder paste 256 seem to be a good and very active n...
- Mar 02, 2005
by
Russ, are you using any reduction on your stencil aperatures...
- Mar 02, 2005
by
adlsmt
I like Alpha Metals OM-5100. Very long stencil life with go...
- Mar 02, 2005
by
We use 10% reductions when either the aspect or area ratio w...
- Mar 02, 2005
by
RDR
we use SENJU M705. type3 solder paste. Has a good shelf life...
- Mar 02, 2005
by
We also use Indium NC-SMQ92J. We do the same as mentioned pe...
- Mar 03, 2005
by
gpaelmo
We use Alpha UP-78 (Older paste formula) and it works well f...
- Mar 04, 2005
by
jbrower