My company just purchased a Vecta (E-vert) wave soldering m...
- May 02, 2000
by
John Sims
Which wave solder flux are you using and what types of preh...
- May 03, 2000
by
C.K.
John - CK can probably help you further once you answer tho...
- May 03, 2000
by
SONO-TEK CORPORATION
We are using NR300F from Alpha. Topside board temp is 220 ...
- May 05, 2000
by
John Sims
I'd have to disagree with the Electrovert applications guy....
- May 05, 2000
by
C.K.
I read my posting again, and it didn't sound right....what ...
- May 05, 2000
by
C.K.
I was running the conveyor at 3.75 when we started the disc...
- May 08, 2000
by
John Sims