I ran six boards with uBGA, and all six have voids 25-30%.
...
- Mar 27, 2000
by
Garo: Voids are primarily process indicators. There is exp...
- Mar 27, 2000
by
davef
Garo,
Minor voiding in Ball Grid Array solder joints is c...
- Mar 29, 2000
by
JAX