I am assembling a board with 2 x ALTERA FineLine PBGA devic...
- Mar 25, 2000
by
Robert,
Have you checked for any form of contamination tha...
- Mar 25, 2000
by
JAX
Dear Robert
The reason for the bridging problem you are ex...
- Mar 27, 2000
by
Mark Alder
Robert: Howya doin' bud?
You say "BGA Shorting!!!" I say...
- Mar 27, 2000
by
davef
Robert,
I think I am late, but better be late than never. ...
- Jun 02, 2000
by
Ravi Bhat
Robert Hutton-Squire