Not all but some new boards we have had solder joint problem...
- Dec 14, 2005
by
snaggletooth
See "black pad" and determine if that's what you have.
...
- Dec 14, 2005
by
RDR
Heavens to Murgatroyd, we agree with Russ that "black pad" c...
- Dec 14, 2005
by
davef
SNAGGLETOOTH HOLDS HIS HANDS UP, HAVING JUST REACHED THE EDG...
- Dec 15, 2005
by
snaggletooth
Snaggie
Oxidized nickel is very tough to solder. Using t...
- Dec 15, 2005
by
davef
i would assume when the PCB planner and customer would speci...
- Dec 16, 2005
by
snaggletooth
Try paste flux instead.... oh yeah.. clean it as soon as it ...
- Dec 16, 2005
by
JAX