Hello,
does anybody have experience in thermosonic gold w...
- Dec 27, 2005
by
Sergey
What's the issue and situation?
...
- Dec 27, 2005
by
davef
I would like to know if ENIG is widely used for the thermoso...
- Dec 28, 2005
by
Sergey
I have lots of experience with thermosonic gold ball bonding...
- Dec 28, 2005
by
You don't TS bond gold wire to nickel [of ENIG] for the same...
- Dec 28, 2005
by
davef
Hello Chris,
To be honest, it's hard to believe you could n...
- Dec 29, 2005
by
Sergey
The paper Dave posted the link for is great. I have to go b...
- Dec 29, 2005
by
Hi, i'm david, new to this forum. Came across your posting a...
- Jan 20, 2006
by
david
Hello David,
No, the capillary does not scrub through the g...
- Jan 20, 2006
by
Sergey
Hello Sergey,
thanks for your input. The capillary i'm usin...
- Jan 22, 2006
by
david